RESEARCH OF ELECTRICAL RESISTANCE AND TEMPERATURE OF THE BEGINNING OF SOFTENING OF CHARGE MIXTURES FOR SMELTING A COMPLEX ALLOY
Mukhambetgaliyev Y.
1 July 2022Faculty of Metallurgy
Metalurgija
2022#61Issue 3-4781 - 784 pp.
The results of the study of the electrical resistance and the temperature of the beginning of softening of high-ash coals of three working seams of the Saryadyr deposit and mixtures of charge materials are presented. The high electrical resistance of the charge in the ore smelting furnace provides a low proportion of charge conductivity and, thereby, contributes to the release of the bulk of the energy in the reaction zone of the furnace, where the metal is formed. The research results showed that the magnitude of the electrical resistance of the charge during non-isothermal heating to high temperatures largely depends on the chemical and mineralogical composition of the charge, as well as on the processes of phase transformations in the sample.
charge mixture , complex alloy , electrical resistance , high-ash coals , temperature
Text of the article Перейти на текст статьи
Abishev Chemical-Metallurgical Institute, Karaganda, Kazakhstan
Abishev Chemical-Metallurgical Institute
10 лет помогаем публиковать статьи Международный издатель
Книга Публикация научной статьи Волощук 2026 Book Publication of a scientific article 2026