The research results are demonstrated on the electrical resistance and beginning softening temperature of the high-ash coals of Saryadyr, Borly and Zhamantuz deposits (Republic of Kazakhstan). Such parameters of the charge in the ore-thermal furnace provide a low fraction of the charge conductivity, and thereby contribute to the release of a main energy fraction in a reaction zone of the furnace where a metal is formed. The research results showed that a value of the electrical resistance of the charge at the non-isothermal heating to the high temperatures depends on the chemical and mineralogical composition of the charges, and on processes of phase transformations in a sample.

Electrical resistance , High-ash coals , Kazakhstan , Non-isothermal heating , Temperature

Text of the article Перейти на текст статьи

Abishev Chemical-Metallurgical Institute, Karaganda, Kazakhstan

Abishev Chemical-Metallurgical Institute

10 лет помогаем публиковать статьи Международный издатель

Книга Публикация научной статьи Волощук 2026 Book Publication of a scientific article 2026